During the processing of methyl methacrylate resin, if the flask is closed prematurely, where is porosity most likely to develop?
Explanation
If the flask is sealed too early during the processing of methyl methacrylate, porosity tends to form in the thickest areas of the resin due to trapped gases and incomplete polymerization.